Issued Patents All Time
Showing 1–25 of 30 patents
| Patent # | Title | Co-Inventors | Date |
|---|---|---|---|
| 12205804 | Silicon sputtering target with special surface treatment and good particle performance and methods of making the same | Yongwen Yuan, Yang Liu, Phil Frausto, Weifang Miao | 2025-01-21 |
| 11062889 | Method of production of uniform metal plates and sputtering targets made thereby | Eduardo del Rio | 2021-07-13 |
| 10655214 | Method of making a tantalum sputter target and sputter targets made thereby | Matthew Fisher, Alex Kuhn | 2020-05-19 |
| 9831073 | Low deflection sputtering target assembly and methods of making same | Yongwen Yuan | 2017-11-28 |
| 9566618 | Silicon sputtering target with special surface treatment and good particle performance and methods of making the same | Yongwen Yuan, Yang Liu, Phil Frausto, Weifang Miao | 2017-02-14 |
| 9546418 | Diffusion-bonded sputter target assembly and method of manufacturing | Weifang Miao, David B. Smathers, Erich Theado, Robert S. Bailey, Jeff Hart | 2017-01-17 |
| 8996944 | Client-server gaming | Ivan M. Ogorodov, Alexander Zelenshikov | 2015-03-31 |
| 8992748 | Sputtering target | Yongwen Yuan, David B. Smathers, Ronald G. Jordan | 2015-03-31 |
| 8506882 | High purity target manufacturing methods | — | 2013-08-13 |
| 8453487 | Circular groove pressing mechanism and method for sputtering target manufacturing | Erich Theado, David B. Smathers | 2013-06-04 |
| 8235277 | Sputtering target assembly and method of making same | Erich Theado | 2012-08-07 |
| 8020748 | Sputtering target assembly and method of making same | Erich Theado | 2011-09-20 |
| 7922881 | Sputtering target with an insulating ring and a gap between the ring and the target | Erich Theado, Harry W. Conard, John Edward Poole | 2011-04-12 |
| 7566415 | Method for manufacturing fully dense metal sheets and layered composites from reactive alloy powders | Vladimir S. Moxson | 2009-07-28 |
| 7146703 | Low temperature sputter target/backing plate method and assembly | — | 2006-12-12 |
| 7114643 | Friction fit target assembly for high power sputtering operation | Harry W. Conard | 2006-10-03 |
| 7063773 | High purity sputter targets with target end-of-life indication and method of manufacture | David B. Smathers, Charles Wickersham, John Edward Poole | 2006-06-20 |
| 6955852 | Method of manufacturing sputter targets with internal cooling channels | — | 2005-10-18 |
| 6872284 | Target and method of optimizing target profile | David B. Smathers, Charles Wickersham, Lin Zhu | 2005-03-29 |
| 6852273 | High-strength metal aluminide-containing matrix composites and methods of manufacture the same | Vladimir S. Moxson | 2005-02-08 |
| 6840427 | Method of manufacturing sputter targets with internal cooling channels | — | 2005-01-11 |
| 6749103 | Low temperature sputter target bonding method and target assemblies produced thereby | Harry W. Conard | 2004-06-15 |
| 6725522 | Method of assembling target and backing plates | Harry W. Conard | 2004-04-27 |
| 6635357 | Bulletproof lightweight metal matrix macrocomposites with controlled structure and manufacture the same | Vladimir S. Moxson | 2003-10-21 |
| 6599466 | Manufacture of lightweight metal matrix composites with controlled structure | Vladimir S. Moxson | 2003-07-29 |