UR

Ulf Rolander

SA Sandvik Ab: 16 patents #8 of 518Top 2%
SA Sandvik Intellectual Property Ab: 5 patents #73 of 773Top 10%
Overall (All Time): #211,013 of 4,157,543Top 6%
21
Patents All Time

Issued Patents All Time

Patent #TitleCo-InventorsDate
7713468 Method of making a sintered body, a powder mixture and a sintered body Jeanette Persson, Leif Dahl, Gerold Weinl 2010-05-11
7645316 Ti(C,N)-(Ti,Nb,W)(C,N)-Co alloy for finishing and semifinishing turning cutting tool applications Marco Zwinkels, Gerold Weinl 2010-01-12
7588621 Ti(C,N)-(Ti,Nb,W)(C,N)-co alloy for milling cutting tool applications Gerold Weinl, Marco Zwinkels 2009-09-15
7332122 Ti(C,N)-(Ti,Nb,W)(C,N)-Co alloy for milling cutting tool applications Gerold Weinl, Marco Zwinkels 2008-02-19
7157044 Ti(C,N)-(Ti,Nb,W)(C,N)-Co alloy for finishing and semifinishing turning cutting tool applications Marco Zwinkels, Gerold Weinl 2007-01-02
6676893 Porous cubic boron nitride based material suitable for subsequent production of cutting tools and method for its production Gerold Weinl 2004-01-13
6344170 Ti(C,N)-(Ti,Ta,W)(C,N)-Co alloy for general finishing cutting tool applications Gerold Weinl, Anders Piirhonen, Marco Zwinkels 2002-02-05
6340445 Ti(C,N)-(Ti,Ta,W)(C,N)-Co alloy for superfinishing cutting tool applications Anders Piirhonen, Marco Zwinkels, Gerold Weinl 2002-01-22
6325838 TI(C, N)--(TI, TA, W) (C, N)--CO alloy for toughness demanding cutting tool applications Gerold Weinl, Anders Piirhonen, Marco Zwinkels 2001-12-04
6290902 Method for producing Ti (C,N)--(Ti,Ta,W) (C,N)--Co alloys for cutting tool applications Marco Zwinkels, Gerold Weinl, Anders Piirhonen 2001-09-18
6287489 Method for making a sintered composite body Gerold Weinl 2001-09-11
6197083 Method for producing titanium-based carbonitride alloys free from binder phase surface layer Gerold Weinl 2001-03-06
6193777 Titanium-based carbonitride alloy with nitrided surface zone Gerold Weinl, Per Lindahl 2001-02-27
6129891 Titanium-based carbonitride alloy with controllable wear resistance and toughness Gerold Weinl, Per Lindahl, Hans-Olof Andren 2000-10-10
6017488 Method for nitriding a titanium-based carbonitride alloy Gerold Weinl, Per Lindahl 2000-01-25
6007909 CVD-coated titanium based carbonitride cutting toll insert Gerold Weinl, Bjorn Henry Lundberg 1999-12-28
6004371 Titanium-based carbonitride alloy with controllable wear resistance and toughness Gerold Weinl, Per Lindahl, Hans-Olof Andren 1999-12-21
5993638 Method for obtaining well-defined edge radii on cutting tool inserts in combination with a high surface finish over the whole insert by electropolishing technique 1999-11-30
5976213 Titanium-based carbonitride alloy with improved thermal shock resistance Gerold Weinl, Camilla Oden, Per Lindahl 1999-11-02
5911867 Method for obtaining a high surface finish on titanium-based coatings by electropolishing Hans J. Johansson 1999-06-15
5591320 Method for obtaining well defined edge radii on cutting tool inserts by electropolishing technique 1997-01-07