Issued Patents All Time
Showing 1–8 of 8 patents
| Patent # | Title | Co-Inventors | Date |
|---|---|---|---|
| 6656296 | Aluminum alloys with optimum combinations of formability, corrosion resistance, and hot workability, and methods of use | Baolute Ren, Subhasish Sircar | 2003-12-02 |
| 6503446 | Corrosion and grain growth resistant aluminum alloy | Baolute Ren, Subhasish Sircar | 2003-01-07 |
| 6458224 | Aluminum alloys with optimum combinations of formability, corrosion resistance, and hot workability, and methods of use | Baolute Ren, Subhasish Sircar | 2002-10-01 |
| 5593516 | High strength, high toughness aluminum-copper-magnesium-type aluminum alloy | — | 1997-01-14 |
| 5512112 | Method of making high strength, high toughness aluminum-copper-magnesium-type aluminum alloy | — | 1996-04-30 |
| 5376192 | High strength, high toughness aluminum-copper-magnesium-type aluminum alloy | — | 1994-12-27 |
| 5273594 | Delaying final stretching for improved aluminum alloy plate properties | — | 1993-12-28 |
| 4391655 | Treatment for the alleviation of high temperature oxidation of aluminum | Michael E. Thurston, Daniel J. Schardein | 1983-07-05 |