4652307 Refining and/or alloying of a 3 percent to 6 percent carbon iron, cobalt, or nickel on a molten silver surface at temperatures 1000.degree. C .degree. C. producing an iron cobalt or nickel powder, or their alloys and a petroleum product 1987-03-24
4406695 Process for producing alloy steel product or iron powder by furnacing ground iron or molten iron on a molten lead bath 1983-09-27