| 11117838 |
Method of making a fiber preform for ceramic matrix composite (CMC) fabrication |
Michael Jacquinto, Stephen Harris, Robert J. Shinavski, Todd Engel |
2021-09-14 |
| 11053801 |
Gas turbine engine composite vane assembly and method for making the same |
Richard C. Uskert, David J. Thomas, Robert J. Shinavski, Adam L. Chamberlain |
2021-07-06 |
| 10941942 |
Retention system for gas turbine engine assemblies |
Ted J. Freeman |
2021-03-09 |
| 10577951 |
Gas turbine engine with dovetail connection having contoured root |
Daniel K. Vetters, Ted J. Freeman, Andrew J. Lazur, Robert J. Shinavski |
2020-03-03 |
| 10174619 |
Gas turbine engine composite vane assembly and method for making same |
Richard C. Uskert, David J. Thomas, Robert J. Shinavski, Adam L. Chamberlain |
2019-01-08 |
| 7988395 |
Mechanical fastener system for high-temperature structural assemblies |
— |
2011-08-02 |
| 7479302 |
Actively-cooled fiber-reinforced ceramic matrix composite rocket propulsion thrust chamber and method of producing the same |
— |
2009-01-20 |
| 6979490 |
Fiber-reinforced ceramic composite material comprising a matrix with a nanolayered microstructure |
— |
2005-12-27 |
| 6783824 |
Actively-cooled fiber-reinforced ceramic matrix composite rocket propulsion thrust chamber and method of producing the same |
— |
2004-08-31 |
| 5558907 |
Pseudo-porous fiber coating for toughened ceramic composite materials and method of producing same |
— |
1996-09-24 |
| 5545435 |
Method of making a toughened ceramic composite comprising chemical vapor deposited carbon and ceramic layers on a fibrous preform |
— |
1996-08-13 |
| 5480707 |
Toughened ceramic composite materials comprising coated refractory fibers in a ceramic matrix wherein the fibers are coated with carbon and an additional coating of ceramic material and carbon mixture |
— |
1996-01-02 |
| 5455106 |
Multilayer fiber coating comprising alternate fugitive carbon and ceramic coating material for toughened ceramic composite materials |
— |
1995-10-03 |
| 5337974 |
Wing pivot structure |
William E. Rumberger |
1994-08-16 |
| 5221578 |
Weak frangible fiber coating with unfilled pores for toughening ceramic fiber-matrix composites |
Harry W. Carpenter, James W. Bohlen |
1993-06-22 |
| 5162271 |
Method of forming a ductile fiber coating for toughening non-oxide ceramic matrix composites |
Harry W. Carpenter, James W. Bohlen |
1992-11-10 |