| 4844951 |
Method for depositing ultrathin laminated oxide coatings |
Vinod K. Sarin, Gilbert Gindraux |
1989-07-04 |
| 4751109 |
A process for depositing a composite ceramic coating on a hard ceramic substrate |
Vinod K. Sarin, Gilbert Gindraux |
1988-06-14 |
| 4749629 |
Ultrathin laminated oxide coatings and methods |
Vinod K. Sarin, Gilbert Gindraux |
1988-06-07 |
| 4745010 |
Process for depositing a composite ceramic coating on a cemented carbide substrate |
Vinod K. Sarin, Gilbert Gindraux |
1988-05-17 |
| 4702970 |
Composite coatings on ceramic substrates |
Vinod K. Sarin |
1987-10-27 |
| 4701384 |
Composite coatings on cemented carbide substrates |
Vinod K. Sarin |
1987-10-20 |
| 4687487 |
Joint implant |
— |
1987-08-18 |
| 4561286 |
Piezoelectric contamination detector |
Jorg Sekler, Alphonse E. Zumsteg |
1985-12-31 |
| 4556098 |
Hot chamber die casting of aluminum and its alloys |
Dominique Hertz |
1985-12-03 |
| 4522453 |
Tribological coatings for the protection of moving machine parts from wear and corrosion |
Johann Lammer, Hans Kocher |
1985-06-11 |
| 4415419 |
Process for producing a corrosion-resistant solid lubricant coating |
Paul Niederhaeuser, Michel Maillat |
1983-11-15 |