Issued Patents All Time
Showing 1–25 of 52 patents
| Patent # | Title | Co-Inventors | Date |
|---|---|---|---|
| 11524334 | Method and apparatus for avoiding erosion in a high pressure die casting shot sleeve for use with low iron aluminum silicon alloys | Steven C. Knickel, Terrance M. Cleary, Kevin R. Anderson, Kevin R. Morasch, Mark R. Witzel | 2022-12-13 |
| 11318530 | Slides and expendable cores for high pressure die cast closed deck engine block | Terrance M. Cleary, Kevin R. Anderson, Alexander K. Monroe, Clayton T. Rasmussen | 2022-05-03 |
| 11090714 | Method and apparatus for avoiding erosion in a high pressure die casting shot sleeve for use with low iron aluminum silicon alloys | Steven C. Knickel, Terrance M. Cleary, Kevin R. Anderson, Kevin R. Morasch, Mark R. Witzel | 2021-08-17 |
| 11047032 | Method for solution heat treating with pressure | Kevin R. Morasch, Kevin R. Anderson, Christopher J. Misorski | 2021-06-29 |
| 10596622 | Slides and expendable cores for high pressure die cast closed deck engine block | Terrance M. Cleary, Kevin R. Anderson, Alexander K. Monroe, Clayton T. Rasmussen | 2020-03-24 |
| 10486229 | Method and apparatus for avoiding erosion in a high pressure die casting shot sleeve for use with low iron aluminum silicon alloys | Steven C. Knickel, Terrance M. Cleary, Kevin R. Anderson, Kevin R. Morasch, Mark R. Witzel | 2019-11-26 |
| 10370742 | Hypereutectic aluminum-silicon cast alloys having unique microstructure | Kevin R. Anderson, Terrance M. Cleary, Alexander K. Monroe | 2019-08-06 |
| 10364484 | Method and alloys for low pressure permanent mold without a coating | Alexander K. Monroe, Kevin R. Anderson, Terrance M. Cleary | 2019-07-30 |
| 10189079 | Slides and expendable cores for high pressure die cast closed deck engine block | Terrance M. Cleary, Kevin R. Anderson, Alexander K. Monroe, Clayton T. Rasmussen | 2019-01-29 |
| 9878367 | Congruent melting salt alloys for use as salt cores in high pressure die casting | Mark T. Degler | 2018-01-30 |
| 9757795 | Method and apparatus for avoiding erosion in a high pressure die casting hot sleeve for use with low iron aluminum silicon alloys | Steven C. Knickel, Terrance M. Cleary, Kevin R. Anderson, Kevin R. Morasch, Mark R. Witzel | 2017-09-12 |
| 9731348 | Method and apparatus for avoiding erosion in a high pressure die casting shot sleeve for use with low iron aluminum silicon alloys | Steven C. Knickel, Terrance M. Cleary, Kevin R. Anderson, Kevin R. Morasch, Mark R. Witzel | 2017-08-15 |
| 9650699 | Nickel containing hypereutectic aluminum-silicon sand cast alloys | Kevin R. Anderson, Terrance M. Cleary, Alexander K. Monroe | 2017-05-16 |
| 9527131 | Congruent melting salt alloys for use as salt cores in high pressure die casting | Mark T. Degler | 2016-12-27 |
| 9114456 | Method and apparatus for avoiding erosion in a high pressure die casting shot sleeve for use with low iron aluminum silicon alloys | Steven C. Knickel, Terrance M. Cleary, Kevin R. Anderson, Kevin R. Morasch, Mark R. Witzel | 2015-08-25 |
| 9114455 | Method and apparatus for avoiding erosion in a high pressure die casting shot sleeve for use with low iron aluminum silicon alloys | Steven C. Knickel, Terrance M. Cleary, Kevin R. Anderson, Kevin R. Morasch | 2015-08-25 |
| 9109271 | Nickel containing hypereutectic aluminum-silicon sand cast alloy | Terrance M. Cleary, Kevin R. Anderson | 2015-08-18 |
| 8220124 | Restoration process for porosity defects in metal cast products | Kevin R. Morasch, Douglas M. Woehlke, Kevin R. Anderson | 2012-07-17 |
| 8074355 | Method for manufacturing a connecting rod for an engine | Terrance M. Cleary | 2011-12-13 |
| 7712216 | Restoration process for porosity defects in metal cast products | Douglas M. Woehlke, Kevin R. Anderson | 2010-05-11 |
| 7666353 | Aluminum-silicon alloy having reduced microporosity | Terrance M. Cleary, Kevin R. Anderson | 2010-02-23 |
| 7494554 | Method for continuous manufacturing of cast articles utilizing one or more fluidized beds for heat treating and aging purposes | Kevin R. Anderson | 2009-02-24 |
| 7347905 | Aluminum-silicon alloy having reduced microporosity and method for casting the same | Terrance M. Cleary, Kevin R. Anderson | 2008-03-25 |
| 7188416 | Restoration process for porosity defects in high pressure die cast engine blocks | Douglas M. Woehlke, Kevin R. Anderson | 2007-03-13 |
| 7100669 | Aluminum-silicon casting alloy having refined primary silicon due to pressure | Terrance M. Cleary | 2006-09-05 |