| 9970079 | Methods for constructing parts using metallic glass alloys, and metallic glass alloy materials for use therewith | Joseph C. Poole, Theodore A. Waniuk, Jeffrey Lee Mattlin, Christopher D. Prest | 2018-05-15 |
| 9962788 | Sub-surface marking of product housings | Matthew S. Scott | 2018-05-08 |
| 9849504 | Metallic glass parts including core and shell | Joseph C. Poole, Theodore A. Waniuk, Jeffrey Lee Mattlin, Christopher D. Prest | 2017-12-26 |
| 9845546 | Sub-surface marking of product housings | — | 2017-12-19 |
| 9839974 | Forming white metal oxide films by oxide structure modification or subsurface cracking | Daniel T. McDonald, Peter N. Russell-Clarke, Masashige Tatebe | 2017-12-12 |
| 9644283 | Laser texturizing and anodization surface treatment | Evans Hankey, Peter N. Russell-Clarke | 2017-05-09 |
| 9568167 | Products with a patterned light-transmissive portion | Jeffrey Howerton, Weixiong Lu | 2017-02-14 |
| 9434197 | Laser engraved reflective surface structures | Peter N. Russell-Clarke | 2016-09-06 |
| 9314871 | Method for laser engraved reflective surface structures | Peter N. Russell-Clarke | 2016-04-19 |
| 9315004 | Accessory units for consumer electronic devices and related assemblies and methods | Santhana K. Balaji, Kevin M. Kenney, Andrew Lauder, Robert Michael Merritt, Samuel G. Smith +4 more | 2016-04-19 |
| 9173336 | Techniques for marking product housings | Rimple Bhatia, Paul Choiniere | 2015-10-27 |
| 9132510 | Multi-step pattern formation | Peter N. Russell-Clarke | 2015-09-15 |
| 9007307 | Method and apparatus for enhancing keycap legend visibility in low light conditions | Ronald J. Moller, John T. Payne, Liliya Lyandres, Kenichi Nakajima, Tsao Lun Chung | 2015-04-14 |
| 8993921 | Method of forming white appearing anodized films by laser beam treatment | Lucy E. Browning, Stephen Brian Lynch, Christopher D. Prest, Peter N. Russell-Clarke, Masashige Tatebe +3 more | 2015-03-31 |
| 8809733 | Sub-surface marking of product housings | Matthew S. Scott | 2014-08-19 |
| 8724285 | Cosmetic conductive laser etching | Kyle Yeates | 2014-05-13 |
| 8723075 | Laser machining of fired ceramic and other hard and/or thick materials | James N. O'Brien, Peter Pirogovsky | 2014-05-13 |
| 8481887 | Method for machining tapered micro holes | Mehmet E. Alpay, Jeffrey Howerton, Ling Wen | 2013-07-09 |
| 8450640 | Panel with micro-hole pattern in a structurally thin portion | Gregg Hardy, Jeffrey Howerton | 2013-05-28 |
| 8394301 | Process for forming panel with an optically transmissive portion and products related thereto | Jeffrey Howerton, Weixiong Lu | 2013-03-12 |
| 8288684 | Laser micro-machining system with post-scan lens deflection | Mehmet E. Alpay, Jeffrey Howerton, Patrick Leonard, David James McKeever | 2012-10-16 |
| 8117744 | Process for forming an isolated electrically conductive contact through a metal package | Jeffrey Howerton | 2012-02-21 |
| 8093532 | Laser machining of fired ceramic and other hard and/or thick materials | James N. O'Brien, Peter Pirogovsky | 2012-01-10 |
| 7968820 | Method of producing a panel having an area with light transmissivity | Gregg Hardy, Jeffrey Howerton | 2011-06-28 |
| 7886437 | Process for forming an isolated electrically conductive contact through a metal package | Jeff Howerton | 2011-02-15 |